STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-9 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarTUFF
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-9 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarTUFF TF 40-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Viscosity 8600 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
8600 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 40

@Time 10.0 sec
40

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 6.69 MPa

@Time 7200 sec
970 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 700 %

@Time 7200 sec
700 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00121 GPa

@Time 7200 sec
0.175 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 22.4 kN/m
128 pli
ASTM D624
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: