Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.69 MPa @Time 7200 sec |
970 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-9 TPE Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tensile Strength at Break | 6.69 MPa @Time 7200 sec |
970 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-9 TPE Product Description: StarTUFF TF 40-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tensile Strength at Break | 6.69 MPa | 970 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |