Saint-Gobain CHR® RU Rulon Film Backing Silicone Adhesive Pressure Sensitive Tape

Category Polymer , Adhesive , Tape , Thermoset , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name CHR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain CHR® RU Rulon Film Backing Silicone Adhesive Pressure Sensitive Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rulon® films offer superior abrasion resistance when compared to conventional PTFE films. Service temperatures range from -100°F to 500°F (-73°C to +260°C). In rotating bearing tests, it provided a 500-fold increase in wear resistance over standard PTFE. Applications include bearing liners, chute and guide rail coverings. This tape uses a silicone adhesive system. Perfect for extreme temperature applications, silicone adhesives perform in continuous operating temperatures from -100°F to 500° (-73°C to 260°C). Silicone-based adhesive systems exhibit good chemical resistance, retain electrical properties, and remove cleanly with little or no residue. All data based on a 0.01 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .008 inches.) Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Elongation at Break 225 %
225 %
Tear Strength 3.51 kN/m
20.0 pli
Initial Tear Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Descriptive Properties Value Comments
Color Rose