Saint-Gobain Chemfab® 10 Tear Resistant PTFE-Coated Glass

Category Ceramic , Glass , Glass Fiber
Manufacturer Saint-Gobain Quartz PLC
Trade Name Chemfab®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemfab® 10 Tear Resistant PTFE-Coated Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gaskets, and other applications where superior tear strength is required. All data based on a 0.01 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 2.0293 g/cc
0.073304 lb/in³
Mechanical Properties Metric English Comments
Tear Strength Test 10
10
Lbs./In. Propagation Tear Strength in fill/transverse direction
10
10
Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 30.7 kN/m
175 pli
Tensile Strength (Fill)
39.4 kN/m
225 pli
Tensile Strength (Warp)
Descriptive Properties Value Comments
Weight (oz/yd^2) 15.2