Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 30.7 kN/m | 175 pli | post cured- 4 hours at 204°C; Die B |
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 30.7 kN/m | 175 pli | post cured- 2 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4720 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 30.7 kN/m | 175 pli | ASTM D624 |
Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material Description: CHO-THERM® 1646 pads offer the best available thermal performance, without the use of grease, in applications where electrical isolation is not required. The low thermal impedance of C.. |
|||
Tear Strength | 30.6 kN/m | 175 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Warp/Longitudinal direction |
Saint-Gobain Chemlam® RL® RL1000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Warp/Longitudinal direction |
Saint-Gobain Chemlam® RL® RL7000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Initial Tear Strength |
Saint-Gobain CHR® 2905-7R Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Initial Tear Strength |
Saint-Gobain CHR® 2915-10 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Initial Tear Strength |
Saint-Gobain CHR® SG03-05(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Initial Tear Strength |
Saint-Gobain CHR® SG03-06(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Initial Tear Strength |
Saint-Gobain CHR® SG05-05(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Initial Tear Strength |
Saint-Gobain CHR® SG05-06(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Warp/Longitudinal direction; ASTM D1000 |
Saint-Gobain COHRlastic® 3010 Low Temperature Flexibility Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7080-1000 TPE Product Description: StarMediflex P 7080-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Tear Resistant PTFE-Coated Glass Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 14 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |
|||
Tear Strength | 30.6 kN/m | 175 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 30.6 kN/m | 175 pli | ISO 34 |
DuPont Vamac® GXF Sample Compound Vulcanizate Slab Cure (5 minutes at 190°C) Without Armeen® 18D Test slab is cured for 5 minutes at 190°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own .. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P Medium Hardness Dense Extrusion FormulationNordel® IP 4725P |
|||
Tear Strength | 30.6 kN/m | 175 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 4770R Heat Resistant Peroxide Compound FormulationNordel® IP 4770R |
|||
Tear Strength | 30.7 kN/m | 175 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Primary PTFE-Coated Glass Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: Ch.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-4070 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma.. |
|||
Tear Strength | 30.7 kN/m | 175 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 10 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.".. |