Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tygon S3â„¢ E-3603 from Saint-Gobain Performance Plastics is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable, flexible tubing products. The bio-based Tygon S3â„¢ line combines the high performance standards customers demand with an eco-friendly tubing design. Crystal-clear and flexible, Tygon S3â„¢ E-3603 non-DEHP tubing delivers the same superior performance you have come to expect, but now in a formulation that contains a non-DEHP plasticizer. Tygon S3â„¢ E-3603 tubing handles most inorganic chemicals found in the laboratory. It is non-oxidizing and non-contaminating, and less permeable than rubber tubing. The glassy-smooth inner bore helps prevent buildup to facilitate cleaning. Coils are marked at 1-foot (30.4 cm) intervals for easy measuring. Applications include analytical instruments, general laboratory, Peristaltic and vacuum pumps, biopharmaceutical, incubators, desiccators, gas lines, and food and beverage. Features and Benefits New bio-based formulation delivers the same excellent performance Outstanding chemical resistance Lot-to-lot consistency for reproducible results Non-oxidizing and non-contaminating Contains no BPA or phthalates Standard sizes available to hold full vacuum at room temperature Smooth, polished inner wall Slips easily over fittings and grips securely for simple lab set-ups Regulatory Information: Tygon S3â„¢ complies with FDA, NSF, 3-A, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EU for many foods and beverages. Tygon S3â„¢ tubing products do not contain chemicals listed in California's Prop 65. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.21 %

@Temperature 22.8 °C,
Time 86400 sec
0.21 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 56

@Time 15.0 sec
56

@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.1 MPa
1750 psi
ASTM D412
Tensile Strength, Yield 4.01 MPa

@Strain 100 %
582 psi

@Strain 100 %
Elongation at Break 425 %
425 %
ASTM D412
Tear Strength 30.3 kN/m
173 pli
ASTM D1004
Compression Set 64 %

@Temperature 70.0 °C,
Time 79200 sec
64 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 95 %
95 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Clear