Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.01 MPa | 581 psi | 200%, post cured- 8 hours at 200°C; ASTM D412 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 4.01 MPa | 582 psi | ASTM D412 |
Polymax® Maxelast® P2765 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.01 MPa | 582 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5243 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 4.01 MPa @Strain 100 % |
582 psi @Strain 100 % |
|
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing Tygon S3™ E-3603 from Saint-Gobain Performance Plastics is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable, flexible tubing products. The bio-ba.. |
|||
Tensile Strength, Yield | 4.01 MPa @Strain 100 % |
582 psi @Strain 100 % |
|
Saint-Gobain Tygon® Transflow S3™ Vacuum Phthalate-free Vacuum and Dairy Tubing, A-24 and A24-C Transflow S3™ Vacuum tubing, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. .. |