Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Tygon® Transflow S3™ Vacuum Phthalate-free Vacuum and Dairy Tubing, A-24 and A24-C

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® Transflow S3™ Vacuum Phthalate-free Vacuum and Dairy Tubing, A-24 and A24-C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Transflow S3â„¢ Vacuum tubing, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Transflow S3â„¢ line combines the high performance standards customers demand with an eco-friendly tubing design. Transflow S3â„¢ Vacuum tubing is ideally suited for supply air transport. The smooth inner surface is less susceptible to particle entrapment, which can restrict air flow, while crystal clarity permits detection of equipment deficiencies such as backflow of milk into the air lines. Transflow S3â„¢ Vacuum tubing is designed to work in tandem with Transflow S3â„¢ M-34-R to provide a vacuum tube and easy fluid flow within the milking process. Every foot of Transflow S3â„¢ Vacuum tubing has been embedded with a trademark blue stripe within the tubing walls. The embedded blue stripe is your assurance of receiving genuine Transflow S3â„¢ tubing, the world's finest raw milk tubing produced specifically for the dairy industry. Applications for this product are raw milk transport lines and dairy processing. Features and Benefits Holds full vacuum at room temperature Will not crack and age like rubber tubing Lightweight and flexible for quick installation Non-wetting properties allow easy cleaning and complete drainage Durability for long and reliable service Contains no BPA or phthalates To be used in conjunction with Transflow S3â„¢ M-34-R tubing Regulatory Information: Transflow S3â„¢ complies with FDA, NSF, 3-A, and Japan Food Sanitation Law # 370/1959 for many foods and beverages. Tygon S3â„¢ tubing products do not contain chemicals listed in California's Prop 65. *For complete compliance information and appropriate use instructions, please refer to the detailed document of compliance. The complete compliance information and use instructions can be found at www.TygonS3.com. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.21 %

@Temperature 22.8 °C,
Time 86400 sec
0.21 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 56

@Time 15.0 sec
56

@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.1 MPa
1750 psi
ASTM D412
Tensile Strength, Yield 4.01 MPa

@Strain 100 %
582 psi

@Strain 100 %
Elongation at Break 425 %
425 %
ASTM D412
Tear Strength 30.3 kN/m
173 pli
ASTM D1004
Compression Set 64 %

@Temperature 70.0 °C,
Time 79200 sec
64 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 95 %
95 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -35.6 °C
-32.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Black
Clear
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved