Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.86 g/cc
1.86 g/cc
ASTM D792
Water Absorption 0.020 %

@Temperature 23.0 °C
0.020 %

@Temperature 73.4 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0080 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Elongation at Break 1.5 %
1.5 %
5 mm/min; ASTM D638
Flexural Strength 177 MPa
25700 psi
2.8 mm/min; ASTM D638
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.392 J/cm

@Thickness 3.17 mm
0.735 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 270 °C

@Thickness 6.40 mm
518 °F

@Thickness 0.252 in
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
50% RH; ASTM D257
Dielectric Constant 5.0

@Frequency 1.00e+6 Hz
5.0

@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.0070

@Frequency 1.00e+6 Hz
0.0070

@Frequency 1.00e+6 Hz
ASTM D150
Users viewing this material also viewed the following: