Polymer Property : Tensile Strength, Yield = 15600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 108 MPa

@Thickness 3.20 mm
15600 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUCON CP2100-KA02 PC+CF
Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical
Tensile Strength, Yield 108 MPa

@Thickness 3.20 mm
15600 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG ..
Tensile Strength, Yield 108 MPa

@Thickness 3.20 mm
15600 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose
Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 108 MPa

@Thickness 3.20 mm
15600 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance
Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical
Tensile Strength, Yield 108 MPa

@Thickness 3.20 mm
15600 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUPOY SC2302 PC+GF30%, High Impact
Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Greene Tweed Arlon® 1000 Polyketone
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Tensile Strength, Yield 108 MPa

@Thickness 3.20 mm
15600 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati..
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Techmer ES HiFill® PA12 GF30 L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF/M36 HS BK 36% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 36% Filler by Weight and Mineral Filler, 36% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Techmer ES Luriblend® PA6/6 GF10 TL10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(5%)Features: Lubricated, Good Wear Resistance, Low Fricti..
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled
Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165BM PPS
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled
Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2165BM PPS
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Tensile Strength, Yield 108 MPa
15600 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Cheng Yu Plastic ML3425 PC, 25% Glass Fiber
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Cheng Yu Plastic NG1200S Nylon 66, 20% Glass Fiber Reinforced
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Cheng Yu Plastic FR200GV20 Flame Retardant Nylon 66, 20% Glass Fiber
Tensile Strength, Yield 108 MPa
15600 psi
ASTM 638
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.