Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 250 °C
16 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 41.2 MPa
5970 psi
50 mm/min; ASTM D638
Elongation at Break 25 %
25 %
50 mm/min; ASTM D638
Flexural Strength 60.8 MPa
8820 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.91 GPa
277 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.94 J/cm

@Thickness 3.17 mm
5.51 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 104 °C
219 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in