Schmolz + Bickenbach UGICHROM 4028 Martensitic Chrome Plated Bar

Category Metal , Ferrous Metal , Martensitic
Manufacturer Schmolz + Bickenbach (Swiss Steel International)
Trade Name UGICHROM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmolz + Bickenbach UGICHROM 4028 Martensitic Chrome Plated Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coefficient; High resistance to wear; Improved corrosion resistance; Micro-fissured chromium (1000 micro-fissures / cm²) guarantees a definitive level of resistance to extreme conditions in severe environments; Improved machinability (up to +20% of productivity); Superior mechanical properties; and High level of geometrical and dimensional precisionInformation provided by Schmolz + Bickenbach
Mechanical Properties Metric English Comments
Hardness, Vickers 900

@Thickness 0.100 mm
900

@Thickness 0.00394 in
Tensile Strength at Break 850 - 1000 MPa
123000 - 145000 psi
Tensile Strength, Yield >= 650 MPa

@Strain 0.200 %
>= 94300 psi

@Strain 0.200 %