Material Notes:
Description: UGISTEAD is a low nickel austenitics with properties equivalent to 4301/4307 (304/304L) in identified media. Grades designed for the food processing and household appliance markets. In certain environments, these grades can replace 1.4301/1.4307 (304L) and still allow an alloy surcharge that is lower and more stable over time. These grades are also interesting for the process industry due to their anti-coking properties.Information provided by Schmolz + Bickenbach
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 17 - 18 %
17 - 18 %
Copper, Cu 2.0 - 3.0 %
2.0 - 3.0 %
Iron, Fe >= 67.87 %
>= 67.87 %
Manganese, Mn 3.0 - 5.0 %
3.0 - 5.0 %
Molybdenum, Mo 0.20 - 0.50 %
0.20 - 0.50 %
Nickel, Ni 3.5 - 4.5 %
3.5 - 4.5 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.010 %
<= 0.010 %