Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott DUROBAX® amber Neutral Glass Tubing

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott DUROBAX® amber Neutral Glass Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neutral glass tubing, chemically highly resistant, with light protection Containers, test tubes, pipettes, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.42 g/cc

@Temperature 25.0 °C
0.0874 lb/in³

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Modulus of Elasticity 71.0 GPa
10300 ksi
Poissons Ratio 0.19
0.19
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 300 °C
3.00 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Thermal Conductivity 1.20 W/m-K

@Temperature 90.0 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 194 °F
Transformation Temperature, Tg 560 °C
1040 °F
ISO 7884-8
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Working Point 1165 °C
2129 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Annealing Point 560 °C
1040 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Optical Properties Metric English Comments
Refractive Index 1.523

@Wavelength 587.6 nm
1.523

@Wavelength 587.6 nm
Electrical Properties Metric English Comments
Volume Resistivity 400000 ohm-cm

@Temperature 350 °C
400000 ohm-cm

@Temperature 662 °F
1.30e+7 ohm-cm

@Temperature 250 °C
1.30e+7 ohm-cm

@Temperature 482 °F
Dielectric Constant 6.3

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
6.3

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Loss Index 0.0107

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
0.0107

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Chemical Properties Metric English Comments
Acid Class, SR 1
1
DIN 12116
Alkali Class, AR 2
2
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 1
ISO 719
Stress-optical Coefficient K (10-6mm2N-1) 2.2
DIN 52314
tk100(°C) 200
Copyright © lookpolymers.com All Rights Reserved