Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include KG2, KG3, KG4, KG1
Physical Properties Metric English Comments
Density 2.53 g/cc
0.0914 lb/in³
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.00 µin/in-°F

@Temperature -22.0 - 158 °F
6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 565 °C
1050 °F
Optical Properties Metric English Comments
Refractive Index 1.52

@Wavelength 587.6 nm
1.52

@Wavelength 587.6 nm
He
1.52

@Wavelength 587.6 nm
1.52

@Wavelength 587.6 nm
He
Transmission, Visible 37 %

@Wavelength 700 nm
37 %

@Wavelength 700 nm
81 - 82 %

@Wavelength 470 - 580 nm
81 - 82 %

@Wavelength 470 - 580 nm
Internal transmittance of 88-89% from 470-580 nm.
IR Transmittance 32 %

@Wavelength 710 nm
32 %

@Wavelength 710 nm
Internal transmittance of 35% at 710 nm.
UV Transmittance <= 0.20 %

@Wavelength 200 - 2900 nm
<= 0.20 %

@Wavelength 200 - 2900 nm
84 %

@Wavelength 380 nm
84 %

@Wavelength 380 nm
Internal transmittance of 91% at 380 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 3
3
Alkali Class, AR 4
4
Stain Resistance Class, FR 0.0
0.0