Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 5.40 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 100 °C
3.00 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1801 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.00 µin/in-°F

@Temperature -22.0 - 158 °F
Schott FG3 Conversion Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BG34, FG13
CTE, linear 5.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.00 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KG4 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG1, KG5
CTE, linear 5.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.00 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KG5 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include KG2, KG3, KG4, KG1
CTE, linear 5.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.00 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KG2 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG1, KG3, KG4, KG5
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 300 °C
3.00 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-KZFS2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.40 µm/m-°C

@Temperature 25.0 - 400 °C
3.00 µin/in-°F

@Temperature 77.0 - 752 °F
CoorsTek ACI-Ni10 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 400 °C
3.00 µin/in-°F

@Temperature 68.0 - 752 °F
CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 200 °C
3.00 µin/in-°F

@Temperature 68.0 - 392 °F
DIN EN 821-1
CeramTec Rubalit® A 1896 Alumina
Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele..
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 200 °C
3.00 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Rubalit® A 1898 Alumina, 98%
Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
Copyright © lookpolymers.com All Rights Reserved