Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott N-LAK33A Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott N-LAK33A Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 4.22 g/cc
0.152 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 740
740
.1/20
Modulus of Elasticity 121 GPa
17500 ksi
Poissons Ratio 0.292
0.292
Shear Modulus 47.0 GPa
6820 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 5.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.22 µin/in-°F

@Temperature -22.0 - 158 °F
7.00 µm/m-°C

@Temperature 20.0 - 300 °C
3.89 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.550 J/g-°C
0.131 BTU/lb-°F
Thermal Conductivity 0.810 W/m-K
5.62 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 669 °C
1240 °F
Optical Properties Metric English Comments
Refractive Index 1.75393

@Wavelength 587.6 nm
1.75393

@Wavelength 587.6 nm
n<sub>d</sub>
1.75737

@Wavelength 546.1 nm
1.75737

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 95 %

@Thickness 10.0 mm,
Wavelength 380 nm
95 %

@Thickness 0.394 in,
Wavelength 380 nm
98.1 %

@Thickness 10.0 mm,
Wavelength 405 nm
98.1 %

@Thickness 0.394 in,
Wavelength 405 nm
99.4 %

@Thickness 10.0 mm,
Wavelength 460 nm
99.4 %

@Thickness 0.394 in,
Wavelength 460 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %

@Thickness 0.394 in,
Wavelength 580 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 39.8 %

@Thickness 10.0 mm,
Wavelength 2500 nm
39.8 %

@Thickness 0.394 in,
Wavelength 2500 nm
99 %

@Thickness 10.0 mm,
Wavelength 1530 nm
99 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 5.3 %

@Thickness 10.0 mm,
Wavelength 300 nm
5.3 %

@Thickness 0.394 in,
Wavelength 300 nm
60.1 %

@Thickness 10.0 mm,
Wavelength 334 nm
60.1 %

@Thickness 0.394 in,
Wavelength 334 nm
92.4 %

@Thickness 10.0 mm,
Wavelength 370 nm
92.4 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 51
51
Alkali Class, AR 1.0
1.0
Stain Resistance Class, FR 1.0
1.0
Descriptive Properties Value Comments
B 0
Climatic Resistance Test CR 1
HG 2
K (10-6mm2/N) 1.49
Phosphate Resistance PR 2
T1013.0 (°C) 667
T107.6 (°C) 744
Users viewing this material also viewed the following: