Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
Schott N-LASF40 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
Schott P-LASF47 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
Schott N-LAF21 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
Schott N-LAK22 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
Schott N-LAK33A Glass Information Provided by SCHOTT North America, Inc. |