Material Notes:
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG665, RG695, RG715, RG780, GG385, RG850, RG1000, WG225, WG280, WG295, WG305, WG320
Physical Properties Metric English Comments
Density 2.94 g/cc
0.106 lb/in³
Thermal Properties Metric English Comments
CTE, linear 9.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.44 µin/in-°F

@Temperature -22.0 - 158 °F
10.7 µm/m-°C

@Temperature 20.0 - 300 °C
5.94 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 569 °C
1060 °F
Glass Temperature Coefficient 0.18
0.18
Optical Properties Metric English Comments
Refractive Index 1.55

@Wavelength 852.1 nm
1.55

@Wavelength 852.1 nm
Cs
1.55

@Wavelength 1014 nm
1.55

@Wavelength 1014 nm
Hg
1.56

@Wavelength 587.6 nm
1.56

@Wavelength 587.6 nm
He
IR Transmittance 90 %

@Wavelength 1000 - 1700 nm
90 %

@Wavelength 1000 - 1700 nm
Internal transmittance of 98-99% from 1000-1900 nm.
UV Transmittance <= 0.0010 %

@Wavelength 200 - 390 nm
<= 0.0010 %

@Wavelength 200 - 390 nm
Internal transmittance of 0.001% from 200-390 nm.
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 4.4
4.4
Alkali Class, AR 1
1
Stain Resistance Class, FR 3
3