Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 570 °C | 1060 °F | ISO 7884-8 |
Schott Glass 8230 Intermediate sealing glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG. |
|||
Transformation Temperature, Tg | 569 °C | 1060 °F | |
Schott N-BAF51 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 569 °C | 1060 °F | |
Schott N-F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 570 °C | 1060 °F | |
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 570 °C | 1060 °F | |
Schott S8807 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 569 °C | 1060 °F | |
Schott RG830 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Transformation Temperature, Tg | 571 °C | 1060 °F | |
Schott RG850 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Transformation Temperature, Tg | 571 °C | 1060 °F | |
Schott RG780 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |