Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.77 g/cc
0.100 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.90 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.39 µin/in-°F

@Temperature -22.0 - 158 °F
8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 603 °C
1120 °F
Optical Properties Metric English Comments
Refractive Index 1.51

@Wavelength 587.6 nm
1.51

@Wavelength 587.6 nm
He
1.57

@Wavelength 365 nm
1.57

@Wavelength 365 nm
Hg
Transmission, Visible <= 0.060 %

@Wavelength 420 - 680 nm
<= 0.060 %

@Wavelength 420 - 680 nm
11 %

@Wavelength 400 nm
11 %

@Wavelength 400 nm
Internal transmittance of 12% at 400 nm
IR Transmittance 42 %

@Wavelength 750 nm
42 %

@Wavelength 750 nm
Internal transmittance of 47% at 750 nm.
UV Transmittance <= 0.40 %

@Wavelength 200 - 280 nm
<= 0.40 %

@Wavelength 200 - 280 nm
76 %

@Wavelength 360 nm
76 %

@Wavelength 360 nm
Internal transmittance of 83% at 360 nm
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0