Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 606 °C | 1120 °F | |
Schott N-PSK53A Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 605 °C | 1120 °F | |
Schott GG435 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG385, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Transformation Temperature, Tg | 605 °C | 1120 °F | |
Schott KG2 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG1, KG3, KG4, KG5 |
|||
Transformation Temperature, Tg | 603 °C | 1120 °F | |
Schott UG1 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |