Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Seals Eastern 5487 Nitrile Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Seals Eastern, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 5487 Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low temperature service Nitrile; plasticizer freeInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.43 MPa
3108 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield 2.68 MPa
388 psi
Stress at Elongation M50; ASTM D412 Method A
6.01 MPa
871 psi
Stress at Elongation M100; ASTM D412 Method A
Elongation at Break 353 %
353 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.01022 GPa
1.483 ksi
ASTM D412 Method A
Shear Modulus 0.00341 GPa
0.494 ksi
ASTM D412 Method A
Secant Modulus 0.009611 GPa
1.394 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -31.7 °C
-25.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 26
Copyright © lookpolymers.com All Rights Reserved