Aaron Industries AAROLENE® ARPE HD 300-2 Black BM High Density Polyethylene, Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPE HD 300-2 Black BM High Density Polyethylene, Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, HDPE Black, Blow Molding GradeFeatures: A high density Polyethylene compound, pre-colored black, specifically designed for all blow molding and pipe applications.
Physical Properties Metric English Comments
Specific Gravity 0.953 g/cc
0.953 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Flexural Modulus 0.814 GPa
118 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.7 °C
170 °F
ASTM D648