Seals Eastern 7017 Ethylene-Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Seals Eastern, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 7017 Ethylene-Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General service EPM.Information provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 57
>= 57
ASTM D2240, Type A
62
62
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 10.56 MPa
>= 1531 psi
ASTM D412 Method A
14.60 MPa
2118 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 0.903 MPa
>= 131 psi
Stress at Elongation M50; ASTM D412 Method A
0.951 MPa
138 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 1.00 MPa
>= 145 psi
Stress at Elongation M100; ASTM D412 Method A
1.23 MPa
178 psi
AVG Stress at Elongation M50; ASTM D412 Method A
1.71 MPa
248 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 232 %
>= 232 %
ASTM D412 Method A
551 %
551 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.00645 GPa
0.935 ksi
ASTM D412 Method A
Shear Modulus 0.00215 GPa
0.312 ksi
ASTM D412 Method A
Secant Modulus 0.00606 GPa
0.879 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -51.1 °C
-60.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 17