Polymer Property : Shear Modulus = 0.312 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.00215 GPa
0.312 ksi
ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.
Shear Modulus 0.00215 GPa
0.312 ksi
ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.