Sekisui PIOCELAN LP-50E Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN LP-50E Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: General molding articles; Packing material for industrial parts; and Returnable containers for electronic parts.Information provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0200 g/cc
0.000723 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.3388 MPa
49.14 psi
ASTM D3575
Elongation at Break 10 %
10 %
ASTM D3575
Flexural Strength 0.2024 MPa
29.36 psi
ASTM D790
Flexural Modulus 0.009687 GPa
1.405 ksi
ASTM D790
Compressive Strength 0.1356 MPa

@Strain 25.0 %
19.67 psi

@Strain 25.0 %
ASTM D3575
0.1938 MPa

@Strain 50.0 %
28.11 psi

@Strain 50.0 %
ASTM D3575
0.4127 MPa

@Strain 75.0 %
59.85 psi

@Strain 75.0 %
ASTM D3575
Compression Set 41.6 %
41.6 %
ASTM D3575
Descriptive Properties Value Comments
Color White
Range of center value of pre-expanded particles 0.15-0.22 in