Flexural Modulus 0.009687 GPa
1.405 ksi
ASTM D790
Sekisui PIOCELAN LP-50E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..