Shakespeare FGN-11 Nylon 6 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare FGN-11 Nylon 6 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For food contact applicationsInformation provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 15 - 45 %
15 - 45 %
Tenacity >= 0.424 N/tex
>= 4.80 g/denier
Thermal Properties Metric English Comments
Shrinkage 4.00 - 9.00 %

@Temperature 177 °C
4.00 - 9.00 %

@Temperature 350 °F