Polymer Property : Tenacity = 0.424 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity >= 0.424 N/tex
>= 4.80 g/denier
Shakespeare FGN-11 Nylon 6 Monofilament
For food contact applicationsInformation provided by Shakespeare Company.
Tenacity 0.424 N/tex
4.80 g/denier
Knot Strength
UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=5)
Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE.
Tenacity 0.424 N/tex
4.80 g/denier
Knot Strength
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.5)
Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE.
Tenacity 0.424 N/tex
4.80 g/denier
Line Strength
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=4.5)
Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE.
Tenacity 0.424 N/tex
4.80 g/denier
Knot Strength
UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=4.8)
Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE.