Shakespeare WN-50 diameter 0.4 mm Nylon Monofilament 610

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WN-50 diameter 0.4 mm Nylon Monofilament 610.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10Moderate ModulusLow moisture regainModerate shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break 434 MPa
63000 psi
Elongation at Yield 7.5 %
7.5 %
at 1.75 g/D
Thermal Properties Metric English Comments
Shrinkage 5.00 %

@Temperature 175 °C
5.00 %

@Temperature 347 °F