Tensile Strength at Break 434 MPa
63000 psi
Shakespeare WN-50 diameter 0.2 mm Nylon Monofilament 610
Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10Moderate ModulusLow moisture regainModerate shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 434 MPa
63000 psi
Shakespeare WN-50 diameter 0.4 mm Nylon Monofilament 610
Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10Moderate ModulusLow moisture regainModerate shrinkage Information provided by Shakespeare Company.