Shakespeare WP-120 diameter 0.7 mm Weft Polyester Monofilament

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WP-120 diameter 0.7 mm Weft Polyester Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterLow modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break 552 MPa
80000 psi
Elongation at Yield 27 %
27 %
at 3 g/D
Thermal Properties Metric English Comments
Shrinkage 5.00 %

@Temperature 200 °C
5.00 %

@Temperature 392 °F