Polymer Property : Tensile Strength at Break = 552 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 380
Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta..
Tensile Strength at Break 552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 452
Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap ..
Tensile Strength at Break 552 MPa
80000 psi
Shakespeare WP-104 diameter 0.2 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentStandard molecular weightPolyesterLow modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 552 MPa
80000 psi
Shakespeare WP-104 diameter 0.4 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentStandard molecular weightPolyesterLow modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 552 MPa
80000 psi
Shakespeare WP-120 diameter 0.2 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterLow modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 552 MPa
80000 psi
Shakespeare WP-120 diameter 0.5 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterLow modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 552 MPa
80000 psi
Shakespeare WP-120 diameter 0.7 mm Weft Polyester Monofilament
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterLow modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 552 MPa
80000 psi
Shakespeare WP-550 diameter 0.5 mm Hydrolytically Stabilized Polyester Yarn
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterHydrolytically stableWarp and weft yarnLow shrinkageLow modulus Information provided by Shakespeare Company.
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Master Bond EP17HT-3 One component, snap-curing epoxy system
Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p..
Tensile Strength at Break 552 - 758 MPa
80100 - 110000 psi
ThyssenKrupp 12Ni5 Structural Steel
5% nickel steel for low temperature service down to -165°FApplication for pressure vessels and tanks for the transportation and storage of ethyleneReference: 5.000 t/y in thicknesses up to 2 in.Hea..
Tensile Strength at Break 552 MPa
80000 psi
Stress relieved
California Fine Wire Copper Clad 1006 Steel (40% Conductivity)
All values may vary dependent on specific design and usage1006 steel core, 99.99% copper cladCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 552 MPa
80000 psi
Annealed
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy
All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 552 MPa
80000 psi
Stress relieved
California Fine Wire Nickel 220 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 552 MPa
80000 psi
Stress relieved
California Fine Wire Nickel 5900 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Carlson 20 Plus Alloy
Carlson C20 Plus is a super-austenitic alloy, developed to provide maximum resistance to corrosion by sulfuric acid. Nickel chromium, molybdenum and copper contribute to the excellent overall resist..
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Carlson 317L 4N Austenitic Stainless Steel
General DescriptionCarlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel a..
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Carlson C 600 Nickel-Chromium-Iron Alloy
Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c..
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Carlson C 600ESR Nickel-Chromium-Iron Alloy
General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell..
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Carlson C 601 Nickel-Chromium-Iron Alloy
General DescriptionCarlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxida..
Tensile Strength at Break 552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is ..
Tensile Strength at Break 552 - 621 MPa
80100 - 90100 psi
Sheet, Cold-rolled & Solution Annealed
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..