Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Polymer DF-202 PTFE Fine Powder

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-202 PTFE Fine Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 004-2003Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Specific Gravity >= 2.20 g/cc
>= 2.20 g/cc
Bulk Density 0.375 - 0.575 g/cc
0.0135 - 0.0208 lb/in³
Particle Size 375 - 675 µm
375 - 675 µm
Mechanical Properties Metric English Comments
Tensile Strength >= 18.6 MPa
>= 2700 psi
Qualified
>= 20.7 MPa
>= 3000 psi
Grade A
>= 24.0 MPa
>= 3480 psi
Excellent
Elongation at Break >= 350 %
>= 350 %
Thermal Properties Metric English Comments
Melting Point 322 - 332 °C
612 - 630 °F
Electrical Properties Metric English Comments
Dielectric Strength <= 2.10 kV/mm
<= 53.3 kV/in
Dissipation Factor 0.00030
0.00030
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
Extrude Pressure (MPa) 5.5-13.9
RR100
For Check Execute according to requirement of HG/T3028-1999
For Process Paste Extrusion
Smoothness & Cleanliness Excellent: White sheet surface, fiber is average, no gravel and metallic powder, even sheet texture < 1 for mechanical impurity (>0.5mm) or organic impurity (>2mm)
Grade A: White sheet surface, fiber is average, no gravel and metallic powder, even sheet texture < 1 for mechanical impurity (>0.5mm) or organic impurity (>2mm)
Qualified: White sheet surface, fiber is average, no gravel and metallic powder, allow 0.5mm organic impurity
Thermal Inst. Index <30
Users viewing this material also viewed the following: