Sharadaa Ceramics PCF80 Precast Prefired Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Sharadaa Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics PCF80 Precast Prefired Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Casting techniques and Pre-fired up to 1450°. Elimination of Casting defects, cracks and voids. Evidencing the Guaranteed data sheet values in the final product.Application Areas:Steel: Well Blocks, Nozzles, EAF Roof, Launders, Impact Pad, Darts Tundish Flow Control Devices, and LancesReheat/Forging furnaces: Hearth Blocks, Burner BlocksFerrous/Non-Ferrous: Launders, Ladles, Doors, Impact Resistant BlocksPetro Chemical: Re-generator Tiles, Mullite Burner BlocksFurnaces: Liner Tiles enabling longer life of Refractories.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
After Drying at 110°C
Porosity 15 %
15 %
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1600 °C
2910 °F
Component Elements Properties Metric English Comments
Al2O3 >= 80 %
>= 80 %
Fe2O3 <= 1.8 %
<= 1.8 %
Descriptive Properties Value Comments
Permanent Linear Change -1.0 - 1.0%
1550°C