Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
MarkeTech Aluminum Oxide Ceramic - Alumina 96% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast ADHESIET 160 Dry Air-Setting Refractory Mortar Description: Adhesiet 160 is an air setting bauxite based mortar with a sodium silicate bond and it is supplied as a dry powder it can be used up to 1600°C.Remarks: The results of the chemical an.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 H SIC GM Dense Refractory Castable Description: This gunning castable has an extremely good thermal shock resistance and very good resistance against aggressive slags. Application among others in the copper industry.Remarks: These va.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 HC Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 H Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics PCF80 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Sharadaa Ceramics MULL Mullite Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Ceramics ECO-20AA Alumina Insulation ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Intermittent |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Zirconia Buster Mat Alumina Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Chosun Refractories 1600BULK Bulk Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | limited |
Chosun Refractories TCH-165Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1600 °C | >= 2910 °F | |
China-Yixing Longly Refractories 99 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | Intermittent |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Zircar Zirconia Buster Blanket Alumina Blanket Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |
|||
Maximum Service Temperature, Air | 1600 °C | 2910 °F | |
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |