Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name Sharada
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 1.00 g/cc

@Temperature 200 °C
0.0361 lb/in³

@Temperature 392 °F
Mechanical Properties Metric English Comments
Compressive Strength 3.43 MPa

@Temperature 800 °C
498 psi

@Temperature 1470 °F
Cold Crushing
4.41 MPa

@Temperature 1300 °C
640 psi

@Temperature 2370 °F
Cold Crushing
4.90 MPa

@Temperature 200 °C
711 psi

@Temperature 392 °F
Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity 0.256 W/m-K

@Temperature 500 °C
1.78 BTU-in/hr-ft²-°F

@Temperature 932 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
Fe2O3 1.0 %
1.0 %
Processing Properties Metric English Comments
Moisture Content 35 - 40 %
35 - 40 %
Recommended