Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 4.90 MPa @Temperature 1300 °C |
711 psi @Temperature 2370 °F |
Cold Crushing |
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Compressive Strength | 4.90 MPa @Temperature 1300 °C |
711 psi @Temperature 2370 °F |
Cold Crushing |
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Compressive Strength | 4.90 MPa @Temperature 110 °C |
711 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Compressive Strength | 4.90 MPa @Temperature 1300 °C |
711 psi @Temperature 2370 °F |
Cold Crushing |
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Compressive Strength | 4.90 MPa @Temperature 200 °C |
711 psi @Temperature 392 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 4.90 MPa @Temperature 800 °C |
711 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 1.2 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 4.90 - 6.86 MPa @Temperature 110 °C, Time 86400 sec |
711 - 996 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories GUN-140L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 7.85 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1140 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-100N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 1420 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 1420 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-135N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT135S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 110 °C, Time 86400 sec |
711 - 2130 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 500 °C, Time 10800 sec |
711 - 2130 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 110 °C, Time 86400 sec |
711 - 2130 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 2130 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1350 °C, Time 10800 sec |
711 - 2130 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 2130 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 110 °C, Time 86400 sec |
711 - 1420 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1350 °C, Time 10800 sec |
711 - 1420 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 9.81 MPa @Temperature 1500 °C, Time 10800 sec |
711 - 1420 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PAC-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |