Sharadaa Ceramics Vacuum Formed Boards

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics Vacuum Formed Boards.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rotary Kiln, Heat Curing and Acid Proof Lining Industry Focuses: Steel, Sponge, Rolling Mills, Coke Oven, Ferrous Foundries, Non-Ferrous, Cement, Petro Chemical, Mineral Processing, Sugar / Paper Mills and Chemical PlantsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Density 0.620 g/cc
0.0224 lb/in³
Thermal Properties Metric English Comments
Thermal Conductivity 0.113 W/m-K

@Temperature 600 °C
0.784 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Maximum Service Temperature, Air 1600 °C
2910 °F