Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones KE-2090-10A/B Self-adhesive LIMS Silicone

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-2090-10A/B Self-adhesive LIMS Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ShinEtsuKE209010 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KE209010 is low enough to allow easy pumping through most injection molding systemsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
Tensile Strength at Break 4.83 MPa
700 psi
Elongation at Break 980 %
980 %
Tear Strength 6.14 kN/m
35.0 pli
Die B
Processing Properties Metric English Comments
Cure Time 15.0 min
0.250 hour
Descriptive Properties Value Comments
Cure Type Press Cure