Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Viscosity 4500 cP
4500 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength 1.40 MPa
203 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 5.00 kV/mm
127 kV/in
Dissipation Factor 0.080

@Frequency 50.0 Hz
0.080

@Frequency 50.0 Hz
Processing Properties Metric English Comments
Cure Time 12.0 min
0.200 hour
Tack Free Time
4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
50% RH
Descriptive Properties Value Comments
Colors Black