Polymer Property : Tensile Strength = 203 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 1.40 MPa
203 psi
ISO 37
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
Tensile Strength 1.40 MPa
203 psi
Test 2; ASTM D412
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi..
Tensile Strength 1.40 MPa
203 psi
Shin-Etsu Silicones KE-3417 Silicone, RTV Adhesive
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 1.40 MPa
203 psi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Tensile Strength >= 1.40 MPa
>= 203 psi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..
Tensile Strength 1.40 MPa

@Strain 20.0 %
203 psi

@Strain 20.0 %
ISO 37
BASF Elastollan S 70 A SPF TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength >= 1.40 MPa
>= 203 psi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..