Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones KEG-2000-30A/B Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KEG-2000-30A/B Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KEG-2000-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesRapid cure time at elevated temperatureLong pot life at room temperatureApplicationsO-ringsDiaphragmsCappingRubber rollersConnector packingsOther electrical partsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 32
32
Tensile Strength 8.501 MPa
1233 psi
Elongation at Yield 750 %
750 %
100% Modulus 0.000703 GPa
0.102 ksi
Tear Strength 25.1 kN/m
143 pli
Compression Set 6.0 %

@Temperature 180 °C,
Time 79200 sec
6.0 %

@Temperature 356 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post Cure
Descriptive Properties Value Comments
Regulatory Testing Class VI, FDA