Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000700 GPa | 0.102 ksi | ASTM D412 |
Network Polymers Softflex® 3300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.000703 GPa | 0.102 ksi | |
Shin-Etsu Silicones KEG-2000-30A/B Elastomer KEG-2000-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy.. |
|||
100% Modulus | 0.000700 GPa | 0.102 ksi | ASTM D638 |
ELASTO UK Dryflex® 650450 TPE, Improved Compression Set and High Temperature Resistance, 45A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
100% Modulus | 0.000700 GPa | 0.102 ksi | ISO 37 |
AlphaGary Evoprene™ 027 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.000700 GPa | 0.102 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 946 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.000700 GPa | 0.102 ksi | ASTM D 638 |
API Megol AM DP2375/30 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.000700 GPa | 0.102 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5685 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |