Sibur 23007-30T Superior Quality Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur 23007-30T Superior Quality Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness.
Physical Properties Metric English Comments
Melt Index of Compound 0.20 - 0.90 g/10 min
0.20 - 0.90 g/10 min
Ash <= 0.035 %
<= 0.035 %
For compounding of stabilization of 16M and painted marks are not normalized
Collected Volatile Condensable Material <= 0.12 %
<= 0.12 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 23.0 MPa
>= 3340 psi
Elongation at Break >= 500 %
>= 500 %
Descriptive Properties Value Comments
Number of Inclusions <3 pcs
Spread Flow Batch Error <±15 %