Material Notes:
With high fluidity of melting, thermal and light resistance for large parts of devices, parts of refrigerators, and for hearing aids. Mark is allowed for contact with food products.
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
Melt Index of Compound 20 - 30 g/10 min
20 - 30 g/10 min
I Preparation
<= 30 g/10 min
<= 30 g/10 min
II Preparation
Mechanical Properties Metric English Comments
Elongation at Break >= 17 %
>= 17 %
II Preparation
>= 20 %
>= 20 %
I Preparation
Izod Impact, Notched (ISO) >= 10.0 kJ/m²
>= 4.76 ft-lb/in²
II Preparation
>= 12.0 kJ/m²
>= 5.71 ft-lb/in²
I preparation
Thermal Properties Metric English Comments
Vicat Softening Point <= 88.0 °C
<= 190 °F
II Preparation
<= 90.0 °C
<= 194 °F
I Preparation
Optical Properties Metric English Comments
Gloss 80 %
80 %
Chemical Properties Metric English Comments
Styrene Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Acrylonitrile Content <.001
Impact Tension Strength >10 MPa
Preparation II
>12 MPa
Preparation I