Silberline 4-Allâ„¢ LEP 20051

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name 4-All™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline 4-Allâ„¢ LEP 20051.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a proprietary inorganic technology to protect against attack by water. 4-Allâ„¢ is applicable to traditional, as well as, lenticular aluminum pigment, offering the coatings formulator maximum flexibility in styling for the automotive and industrial coating markets.Applications: General Industrial
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
Bulk Factor 0.091
0.091
Volatiles 53.5 %
53.5 %
Particle Size 19 µm
19 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.01% retained
Descriptive Properties Value Comments
Category Non-leafing
Solvents Propylene Glycol Ether