Silberline Sparkle Silver® Premier 55

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver® Premier
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® Premier 55.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Silver Dollar" technology provides whiter, brighter, and cleaner polychromatic effects.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.86 g/cc
1.86 g/cc
Bulk Factor 0.065
0.065
Volatiles 20 %
20 %
Particle Size 34 µm
34 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash