Material Notes:
Stamford O is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is an economical grade with cornflake geometry and wide particle size distribution range. This grade can be used with chromatic pigments to produce colored metallic effects.Applications: General Industrial
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Bulk Factor 0.081
0.081
Volatiles 35 %
35 %
Particle Size 17 µm
17 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Aromatic